Polymer Property : Dielectric Strength = 15.2 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 0.600 kV/mm

@Thickness >=3.00 mm
15.2 kV/in

@Thickness >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2
Elektro-Isola Etronax MMF Phenolic, Cotton Fabric Reinforcement, Brown, Sheets
Description: Reinforced with a finer cotton fabric than Etronax MF. Also well suited in particular for small components which are subject to mechanical load and wear. Can be machined to finer tolera..
Dielectric Strength 0.600 kV/mm

@Thickness >=3.00 mm
15.2 kV/in

@Thickness >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2
Elektro-Isola Etronax MMMF Phenolic, Cotton Fabric Reinforcement, Light Brown, Sheets
Description: Friction reducing material consisting of phenolic resin and a very fine cotton fabric. Exclusively for mechanical applications. Good dry-run properties but can be lubricated with oil, g..
Dielectric Strength 0.600 kV/mm

@Thickness >=3.00 mm
15.2 kV/in

@Thickness >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2
Elektro-Isola Etronax MMMF PTFE Phenolic, Cotton Fabric Reinforcement, Light Brown, Sheets
Description: Friction reducing material consisting of phenolic resin with PTFE (Teflon®) and a very fine cotton fabric. Exclusively for mechanical applications. Very good dry run properties. Well s..
Dielectric Strength 0.600 kV/mm

@Thickness >=3.00 mm
15.2 kV/in

@Thickness >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2
Elektro-Isola Etronit IIQ S AL Phenolic, Paper Reinforcement, Black with foil, Sheets
Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Material is black throughout. Elegant surface finish combined with good ..
Dielectric Strength 0.600 kV/mm

@Thickness >=3.00 mm
15.2 kV/in

@Thickness >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2
Elektro-Isola Etronit IIQ S Phenolic, Paper Reinforcement, Black, Sheets
Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Material is black throughout. Elegant surface finish combined with good ..
Dielectric Strength 0.600 kV/mm

@Thickness >=3.00 mm
15.2 kV/in

@Thickness >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2
Elektro-Isola Etronit MBM Phenolic/melamine, Paper Reinforcement, Grey/also other Colors, Sheets
Description: The surfaces consist of melamine, which ensures a scratch-resistant, tracking-resistant surface. The surfaces are grey as standard, but other colors can be selected from the color chart..