Polymer Property : Dielectric Strength = 19.0 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 19.0 kV/mm

@Thickness 3.20 mm
483 kV/in

@Thickness 0.126 in
Conditioned; ASTM D149
Solvay Specialty Polymers Amodel® AE-4133 Polyphthalamide (PPA)  (Unverified Data**)
Amodel AE-4133 is a 33% glass reinforced, hot-water moldable polyphthalamide (PPA) designed to work in the modern automotive electrical environment. This grade features a high heat deflection temper..
Dielectric Strength 19.0 kV/mm

@Thickness 3.20 mm
483 kV/in

@Thickness 0.126 in
ASTM D149
Solvay Specialty Polymers Amodel® AE-4133 Polyphthalamide (PPA)  (Unverified Data**)
Amodel AE-4133 is a 33% glass reinforced, hot-water moldable polyphthalamide (PPA) designed to work in the modern automotive electrical environment. This grade features a high heat deflection temper..
Dielectric Strength 19.0 kV/mm

@Thickness 3.00 mm
483 kV/in

@Thickness 0.118 in
ASTM D149
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been formula..
Dielectric Strength 19.0 kV/mm

@Thickness 1.00 mm
483 kV/in

@Thickness 0.0394 in
short time; IEC 60243-1
SABIC Innovative Plastics Valox® 420 PBT
30% GR, excellent strength, stiffness and dimensional stability. High heat resistance. Appliance handles, spotlights, electric motors, connectors.
Dielectric Strength 19.0 kV/mm

@Thickness 1.00 mm
483 kV/in

@Thickness 0.0394 in
short time; IEC 60243-1
SABIC Innovative Plastics Valox® 420 PBT (Europe-Africa-Middle East)
VALOX 420 is a 30% glass fiber reinforced PBT injection moulding resin with excellent mechanical and thermal properties. Applications: appliance handles, spotlights, electric motors.
Dielectric Strength 19.0 kV/mm

@Thickness 3.20 mm
483 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® 420SE0 PBT
30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc
Dielectric Strength 19.0 kV/mm

@Thickness 3.20 mm
483 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® 420SE0 PBT (Asia Pacific)
30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc
Dielectric Strength 19.0 kV/mm

@Thickness 3.20 mm
483 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® 420SE0 PBT (Europe-Africa-Middle East)
30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc
Dielectric Strength 19.0 kV/mm

@Thickness 3.20 mm
483 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® 420SE0U PBT
PBT, 30% Glass Reinforced, Flame Retardant UL94 V-0/5VA rated, UV-Stabilized
Dielectric Strength 19.0 kV/mm

@Thickness 3.20 mm
483 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® 4631 PBT (Europe-Africa-Middle East)
VALOX 4631 is a 30% glass reinforced, flame retarded PBT injection moulding resin with good electrical properties and excellent mechanical properties.
Dielectric Strength 19.0 kV/mm

@Thickness 1.60 mm
483 kV/in

@Thickness 0.0630 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® 865 PBT (Europe-Africa-Middle East)
VALOX 865 is a 30% glass fibre reinforced, non blooming flame retardant PBT+PET blend with an excellent surface appearance. Applications: External housings, steam irons, appliance housings and light..
Dielectric Strength 19.0 kV/mm

@Thickness 1.60 mm
483 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® 865 PBT (Europe-Africa-Middle East)
VALOX 865 is a 30% glass fibre reinforced, non blooming flame retardant PBT+PET blend with an excellent surface appearance. Applications: External housings, steam irons, appliance housings and light..
Dielectric Strength 19.0 kV/mm

@Thickness 1.00 mm
483 kV/in

@Thickness 0.0394 in
short time; IEC 60243-1
SABIC Innovative Plastics Valox® DR48 - CS1049 PBT (Europe-Africa-Middle East)
VALOX DR48 is a 15 % glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot..
Dielectric Strength 19.0 kV/mm

@Thickness 1.00 mm
483 kV/in

@Thickness 0.0394 in
short time; IEC 60243-1
SABIC Innovative Plastics Valox® DR48 PBT (Europe-Africa-Middle East)
VALOX DR48 is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromoto..
Dielectric Strength 19.0 kV/mm

@Thickness 1.00 mm
483 kV/in

@Thickness 0.0394 in
short time; IEC 60243-1
SABIC Innovative Plastics Valox® DR48V PBT (Europe-Africa-Middle East)
VALOX DR48V is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot..
Dielectric Strength 19.0 kV/mm

@Thickness 3.20 mm
483 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® ENH4550 PBT (Asia Pacific)
25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin.
Dielectric Strength 19.0 kV/mm

@Thickness 3.20 mm
483 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® ENH4550 PBT (Asia Pacific)
25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin.
Dielectric Strength 19.0 kV/mm

@Thickness 3.20 mm
483 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® ENH4550 PBT (Europe-Africa-Middle East)
25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin.
Dielectric Strength 19.0 kV/mm

@Thickness 3.20 mm
483 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® ENH4550 PBT (Europe-Africa-Middle East)
25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin.
Dielectric Strength 19.0 kV/mm

@Thickness 3.20 mm
483 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East)
Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend
Dielectric Strength 19.0 kV/mm

@Thickness 3.20 mm
483 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East)
Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend
Dielectric Strength 19.0 kV/mm

@Thickness 3.20 mm
483 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics Xenoy® 6620 PBT+PC
PBT+PC, Unreinforced, impact modified thermoplastic alloy. Outstanding impact at low temperature
Dielectric Strength 19.0 kV/mm

@Thickness 3.20 mm
483 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Xenoy® 6620 PBT+PC
PBT+PC, Unreinforced, impact modified thermoplastic alloy. Outstanding impact at low temperature
Dielectric Strength 19.0 kV/mm

@Thickness 1.00 mm
483 kV/in

@Thickness 0.0394 in
short time; IEC 60243-1
SABIC Innovative Plastics Xenoy® CL200 PBT+PC (Europe-Africa-Middle East)
XENOY CL200 is a semi-crystalline thermoplastic blend, specially developed to obtain good low temperature impact strength combined with excellent chemical resistance to occasional solvent and gasoli..
Dielectric Strength 19.0 kV/mm

@Thickness 2.00 mm
483 kV/in

@Thickness 0.0787 in
Practical Use (Water Absorption 2.0%); ASTM-D149
Toyobo GLAMIDE® T-403 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Dielectric Strength 19.0 kV/mm

@Thickness 2.00 mm
483 kV/in

@Thickness 0.0787 in
Practical Use (Water Absorption 1.6%); ASTM-D149
Toyobo GLAMIDE® TY-181GC Nylon/Elastomer
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Dielectric Strength 19.0 kV/mm

@Thickness 3.20 mm,
Temperature 150 °C
483 kV/in

@Thickness 0.126 in,
Temperature 302 °F
Short Time; ASTM D149
DuPont Performance Polymers Rynite® 830ER NC010 PET
Rynite® 830ER is 30% glass reinforced with excellent high temperature dielectric properties. Class H (180C).Information provided by DuPont Performance Polymers
Dielectric Strength 19.0 kV/mm

@Thickness 3.20 mm,
Temperature 95.0 °C
483 kV/in

@Thickness 0.126 in,
Temperature 203 °F
Short Time; ASTM D149
DuPont Performance Polymers Rynite® 830ER NC010 PET
Rynite® 830ER is 30% glass reinforced with excellent high temperature dielectric properties. Class H (180C).Information provided by DuPont Performance Polymers