Polymer Property : Dielectric Strength = 2.00 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 2.00 kV/mm

@Frequency 60.0 Hz
50.8 kV/in

@Frequency 60.0 Hz
short time, wet; ASTM D149
Sumitomo Bakelite North America RX® 525 Cellulose Reinforced Phenolic Novolac
RXÂ 525 is a cellulose fiber reinforced phenolic novolac molding compound. This material is recommended for parts requiring moderate toughness. It is designed to meet the requirements of ASTM D-594..
Dielectric Strength 2.00 kV/mm

@Thickness 3.00 mm
50.8 kV/in

@Thickness 0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60245-1; IEC/EN 60893-2 6.1.3.1
Elektro-Isola Etronax MMF Phenolic, Cotton Fabric Reinforcement, Brown, Sheets
Description: Reinforced with a finer cotton fabric than Etronax MF. Also well suited in particular for small components which are subject to mechanical load and wear. Can be machined to finer tolera..
Dielectric Strength 2.00 kV/mm

@Thickness 3.00 mm
50.8 kV/in

@Thickness 0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60245-1; IEC/EN 60893-2 6.1.3.1
Elektro-Isola Etronax MMMF Phenolic, Cotton Fabric Reinforcement, Light Brown, Sheets
Description: Friction reducing material consisting of phenolic resin and a very fine cotton fabric. Exclusively for mechanical applications. Good dry-run properties but can be lubricated with oil, g..
Dielectric Strength 2.00 kV/mm

@Thickness 3.00 mm
50.8 kV/in

@Thickness 0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60245-1; IEC/EN 60893-2 6.1.3.1
Elektro-Isola Etronax MMMF PTFE Phenolic, Cotton Fabric Reinforcement, Light Brown, Sheets
Description: Friction reducing material consisting of phenolic resin with PTFE (Teflon®) and a very fine cotton fabric. Exclusively for mechanical applications. Very good dry run properties. Well s..
Dielectric Strength 2.00 kV/mm

@Thickness >=3.00 mm
50.8 kV/in

@Thickness >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2
Elektro-Isola G-Etronax SI Silicone, Glass Fabric Reinforcement, White, Sheets
Description: Electrical and electrotechnical applications. Suitable as high-frequency insulation on account of its dielectric loss. Used as, among other things, an insulation material in large induc..