Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 21.3 kV/mm @Thickness 1.57 mm |
540 kV/in @Thickness 0.0620 in |
Condition - A |
Industrial Laminates/Norplex NP190 Synthetic Fabric
(discontinued **) Description: Aramid fabric material with a high performance phenolic resin matrix. Excellent electrical and mechanical properties at elevated temperatures, and in adverse environments. Applications .. |