Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® 201R PC (Europe-Africa-Middle East) LEXAN 201R is a high viscosity multi purpose grade and contains a release agent to ensure easy processing. This grade is UL94-V2 at 0.8 mm approved. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® 241RX PC (Europe-Africa-Middle East) LEXAN 241RX is a medium viscosity multi purpose grade and contains a release agent to ensure easy processing. This grade is UL94-V2 at 0.75 mm and allows for the molder to use up to 50 percent regri.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® HP1R PC (Europe-Africa-Middle East) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount o.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
ASTM D149 |
SABIC Innovative Plastics Lexan® IR1810 PC (Europe-Africa-Middle East) IR1810 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics Lexan® IR1810 PC (Europe-Africa-Middle East) IR1810 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
ASTM D149 |
SABIC Innovative Plastics Lexan® IR2110 PC (Europe-Africa-Middle East) IR2110 resin is a medium-high flow (MFR = 15 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics Lexan® IR2110 PC (Europe-Africa-Middle East) IR2110 resin is a medium-high flow (MFR = 15 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
ASTM D149 |
SABIC Innovative Plastics Lexan® IR2240 PC (Europe-Africa-Middle East) IR 2240 resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. Food contact approved |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
ASTM D149 |
SABIC Innovative Plastics Lexan® PC0700 PC (Asia Pacific) PC0700 resin is a low flow (MFR = 7 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. It.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics Lexan® PC1000 PC (Europe-Africa-Middle East) PC1000 resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rele.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics Lexan® PC2200 PC (Asia Pacific) PC2200 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 2.00 mm, Temperature 23.0 °C |
686 kV/in @Thickness 0.0787 in, Temperature 73.4 °F |
IEC 60243-1 |
DuPont Performance Polymers Sorona® 3015GV NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® 3015GV NC010 is a 15% glass reinforced PTT resin containing 31% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness and sur.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® 221R PC (Europe-Africa-Middle East) LEXAN 221R is a low viscosity multi purpose grade and contains a release agent to ensure easy processing. This grade is UL94-V2 at 0.4 mm approved. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® ML3021A PC (Europe-Africa-Middle East) LEXAN ML3021A is a high viscosity, UV stabilised grade especially designed for injection blow moulding and profile extrusion.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regi.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics PC0700 PC (Asia Pacific) PC0700 resin is a low flow (MFR = 7 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
ASTM D149 |
SABIC Innovative Plastics PC0703 PC (Europe-Africa-Middle East) PC0703 resin is a low flow (MFR = 7 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product designed for use in the extrusion market. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
ASTM D 149 |
SABIC Innovative Plastics PC0800 PC PC0800 resin is a low flow (MFR = 8 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
ASTM D 149 |
SABIC Innovative Plastics PC1000 PC (Europe-Africa-Middle East) PC1000 resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold r.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics PC1000R PC (Asia Pacific) PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics PC1003R PC (Asia Pacific) PC1003R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics PC1800 PC (Asia Pacific) PC1800 resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold .. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics PC1800 PC (Europe-Africa-Middle East) PC1800 resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold .. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
ASTM D149 |
SABIC Innovative Plastics PC2200 PC (Asia Pacific) PC2200 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
ASTM D149 |
SABIC Innovative Plastics PC2200 PC (Europe-Africa-Middle East) PC2200 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics PC2200R PC (Asia Pacific) PC2200R resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplied by S.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics PC2200R PC (Europe-Africa-Middle East) PC2200R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics ULTEM 2100R PEI (Europe-Africa-Middle East) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 0.800 mm |
686 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 8032U PBT+PET (Europe-Africa-Middle East) VALOX 8032U is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. Applications: appliance housings, door handles, mirror brackets. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics PC1800R PC (Europe-Africa-Middle East) PC1800R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
ASTM D 149 |
SABIC Innovative Plastics PC2200 PC PC2200 resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T.. |