Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Europe-Africa-Middle East) CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of propertiesThis data was supplied by.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® 2014R PC (Europe-Africa-Middle East) LEXAN 2014R is a medium viscosity flame retardant grade, This material contains a release agent to ensure easy processing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region... |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® 2034 PC (Europe-Africa-Middle East) LEXAN 2034 is a medium viscosity flame retardant grade. The material is UV-stabilized. Glow wire at 960C also satisfies EDF spec HN 60-S-02. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® HP1R PC (Europe-Africa-Middle East) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount o.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
ASTM D149 |
SABIC Innovative Plastics Lexan® IR2840 PC (Europe-Africa-Middle East) IR 2840 resin is a medium-low flow (MFR = 6.5 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. Food contact approved.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
ASTM D149 |
SABIC Innovative Plastics Lexan® PC1000 PC (Europe-Africa-Middle East) PC1000 resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rele.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics Lexan® PC1000 PC (Europe-Africa-Middle East) PC1000 resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rele.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics Lexan® VR1820 PC (Europe-Africa-Middle East) VR1820 resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics PC0700 PC (Asia Pacific) PC0700 resin is a low flow (MFR = 7 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics PC0700 PC (Europe-Africa-Middle East) PC0700 resin is a low flow (MFR = 7 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics PC0700 PC (Europe-Africa-Middle East) PC0700 resin is a low flow (MFR = 7 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. It.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
ASTM D 149 |
SABIC Innovative Plastics PC1000 PC (Asia Pacific) PC1000 resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold r.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
ASTM D 149 |
SABIC Innovative Plastics PC1000R PC (Asia Pacific) PC1000R resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplie.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
ASTM D149 |
SABIC Innovative Plastics PC1000R PC (Asia Pacific) PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
ASTM D149 |
SABIC Innovative Plastics PC1000R PC (Europe-Africa-Middle East) PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics PC1500 PC (Europe-Africa-Middle East) PC1500 resin is a medium-high flow (MFR = 15 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
ASTM D 149 |
SABIC Innovative Plastics PC1800 PC (Europe-Africa-Middle East) PC1800 resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold .. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics PC1800R PC PC1800R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was suppli.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics PC1803R PC PC1803R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics PC2200 PC (Asia Pacific) PC2200 resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics PC2200 PC (Asia Pacific) PC2200 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
ASTM D149 |
SABIC Innovative Plastics PC2203R PC (Asia Pacific) PC2203R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics PC2203R PC (Asia Pacific) PC2203R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics PC2203R PC (Europe-Africa-Middle East) PC2203R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Ultem 2110F PEI (Europe-Africa-Middle East) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be supported with biocompatibility informati.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 0.800 mm |
686 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
ASTM D149 |
SABIC Innovative Plastics PC1800 PC (Asia Pacific) PC1800 resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
ASTM D149 |
SABIC Innovative Plastics PC1800R PC (Europe-Africa-Middle East) PC1800R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
IEC 60243-1 |
SABIC Innovative Plastics PC1800R PC (Europe-Africa-Middle East) PC1800R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |