Electrical Properties Metric English Comments
Insulation Resistance 10.0 - 1.00e+8 ohm
10.0 - 1.00e+8 ohm
Average value: 2.63e+6 ohm Grade Count:22
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler". Specific grades with carbon fiberr content be..
Insulation Resistance 100 - 1.00e+8 ohm
100 - 1.00e+8 ohm
Average value: 1.11e+7 ohm Grade Count:9
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu..
Insulation Resistance 100000 - 1.00e+8 ohm
100000 - 1.00e+8 ohm
Lehmann & Voss LUVOCOM® 1105-8169 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista..
Insulation Resistance 1.00e+6 - 1.00e+8 ohm
1.00e+6 - 1.00e+8 ohm
Lehmann & Voss LUVOCOM® 1301-8367 PPS, linear, with CNT
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. ..
Insulation Resistance 10000 - 1.00e+8 ohm
10000 - 1.00e+8 ohm
Lehmann & Voss LUVOCOM® 20-8244 Polyphthalamide, with carbon fiber and glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
Insulation Resistance 10000 - 1.00e+8 ohm
10000 - 1.00e+8 ohm
Lehmann & Voss LUVOCOM® 65-7311 PP-copolymer, with carbon fiber
Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided by Lehmann & ..