Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 10.0 - 1.00e+11 ohm | 10.0 - 1.00e+11 ohm | Average value: 4.63e+9 ohm Grade Count:24 |
Overview of materials for Acetal Copolymer, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Insulation Resistance | 10.0 - 1.00e+8 ohm | 10.0 - 1.00e+8 ohm | Average value: 2.63e+6 ohm Grade Count:22 |
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler". Specific grades with carbon fiberr content be.. |
|||
Insulation Resistance | 10.0 - 1.00e+14 ohm | 10.0 - 1.00e+14 ohm | Average value: 4.13e+12 ohm Grade Count:25 |
Overview of materials for Nylon 12 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en.. |
|||
Insulation Resistance | 10.0 - 1.00e+10 ohm | 10.0 - 1.00e+10 ohm | Average value: 7.22e+8 ohm Grade Count:14 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu.. |