Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 36500 V | 36500 V | IPC TM-650 2.5.6 |
Arlon MULTICLAD™ HF Halogen-Free Low-Loss Laminate and Prepreg System MULTICLAD™ HF represents the next generation low-loss thermoset and prepreg system for high-speed and high-frequency printed circuit boards. This technology combines a low-loss, high reliability t.. |