Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | >= 50000 V | >= 50000 V | IPC-TM-650.2.5.6 |
Park Electrochemical Nelco® N4000-7 SI® FR-4 Epoxy Laminate and Prepreg The Nelco® N4000-7 low-CTE epoxy laminate and prepreg system is a cost-effective solution for use in a broad range of multilayer PCB designs requiring low Z-axis expansion, excellent thermal stabil.. |
|||
Dielectric Breakdown | >= 50000 V | >= 50000 V | IPC-TM-650.2.5.6 |
Park Electrochemical Nelco® N5000-30/32 BT Epoxy Package The Nelco N5000-30 prepreg and N5000-32 laminate BT epoxy materials are designed specifically to meet or exceed new and emerging chippackaging requirements. The primary applications of these materia.. |
|||
Dielectric Breakdown | >= 50000 V | >= 50000 V | IPC-TM-650.2.5.6 |
Park Electrochemical Nelco® N8000Q Cyanate Ester Epoxy Laminate and Prepreg The Nelco N8000 is a high-Tg cyanate ester laminate and prepreg system that provides superior performance and product integrity and is ideal for board designs with higher layer counts, finer lines a.. |
|||
Dielectric Breakdown | 50000 V | 50000 V | IPC-TM-650.2.5.6 |
Park Electrochemical Nelco® NX9240 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Dielectric Breakdown | 50000 V | 50000 V | IPC-TM-650.2.5.6 |
Park Electrochemical Nelco® NX9250 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Dielectric Breakdown | 50000 V | 50000 V | IPC-TM-650.2.5.6 |
Park Electrochemical Nelco® NX9270 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Dielectric Breakdown | 50000 V | 50000 V | IPC-TM-650.2.5.6 |
Park Electrochemical Nelco® NX9294 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Dielectric Breakdown | 50000 V | 50000 V | IPC-TM-650.2.5.6 |
Park Electrochemical Nelco® NX9300 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Dielectric Breakdown | 50000 V | 50000 V | IPC-TM-650.2.5.6 |
Park Electrochemical Nelco® NX9320 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Dielectric Breakdown | 50000 V | 50000 V | IPC-TM-650.2.5.6 |
Park Electrochemical Nelco® NY9208 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Dielectric Breakdown | 50000 V | 50000 V | IPC-TM-650.2.5.6 |
Park Electrochemical Nelco® NY9233 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Dielectric Breakdown | >= 50000 V | >= 50000 V | IPC-TM-650.2.5.6 |
Park Electrochemical Nelco® N4000-12 SI® High Speed/Low Loss, CAF Resistant Laminate and Prepreg The Nelco® N4000-12 series is an enhanced epoxy resin system designed for use in high speed, low loss applications requiring thermal stability, excellent signal speed and CAF resistance.Key Feature.. |
|||
Dielectric Breakdown | >= 50000 V | >= 50000 V | IPC-TM-650.2.5.6 |
Park Electrochemical Nelco® N4000-13 High-Speed Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-13 series is an enhanced epoxy resin system engineered to provide both outstanding thermal and high signal speed / low signal loss properties. N4000-13 SI® is excellent for applic.. |
|||
Dielectric Breakdown | >= 50000 V | >= 50000 V | IPC-TM-650.2.5.6 |
Park Electrochemical Nelco® N4000-13 SI® High-Speed Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-13 series is an enhanced epoxy resin system engineered to provide both outstanding thermal and high signal speed / low signal loss properties. N4000-13 SI® is excellent for applic.. |
|||
Dielectric Breakdown | >= 50000 V | >= 50000 V | IPC-TM-650.2.5.6 |
Park Electrochemical Nelco® N4000-2 Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-2 is the most established material of Nelco’s product line. This multifunctional epoxy laminate and prepreg system has a long history of use and one of the broadest operating and .. |
|||
Dielectric Breakdown | >= 50000 V | >= 50000 V | IPC-TM-650.2.5.6 |
Park Electrochemical Nelco® N4000-7 EF® Halogen-Free Epoxy The Nelco® N4000-7 EF® series of laminates and prepregs is a total environmental solution. This advanced halogen-free resin system provides superior CAF resistance for high temperature, lead-free .. |
|||
Dielectric Breakdown | >= 50000 V | >= 50000 V | IPC-TM-650.2.5.6 |
Park Electrochemical Nelco® N4000-7 FR-4 Epoxy Laminate and Prepreg The Nelco® N4000-7 low-CTE epoxy laminate and prepreg system is a cost-effective solution for use in a broad range of multilayer PCB designs requiring low Z-axis expansion, excellent thermal stabil.. |
|||
Dielectric Breakdown | >= 50000 V | >= 50000 V | IPC-TM-650.2.5.6 |
Park Electrochemical Nelco® N4350-13 RF Microwave Performance, Modified Epoxy The Nelco N4350-13 RF and N4380-13 RF series are enhanced epoxy resin systems specifically engineered to provide a unique solution for design applications that demand outstanding thermal properties,.. |
|||
Dielectric Breakdown | >= 50000 V | >= 50000 V | IPC-TM-650.2.5.6 |
Park Electrochemical Nelco® N4380-13 RF Microwave Performance, Modified Epoxy The Nelco N4350-13 RF and N4380-13 RF series are enhanced epoxy resin systems specifically engineered to provide a unique solution for design applications that demand outstanding thermal properties,.. |
|||
Dielectric Breakdown | >= 50000 V | >= 50000 V | IPC-TM-650.2.5.6 |
Park Electrochemical Nelco® N7000-1 Polyimide Laminate and Prepreg The Nelco N7000-1 series of polyimide laminate and prepreg has alow Z-axis expansion and high Tg offering PCB manufacturers consistent board performance and reliability. N7000-1 is a good choice for.. |
|||
Dielectric Breakdown | >= 50000 V | >= 50000 V | IPC-TM-650.2.5.6 |
Park Electrochemical Nelco® N7000-2 HT/N7000-3 Toughened Polyimide Laminate and Prepreg The Nelco N7000-2 HT laminate and N7000-3 prepreg are a series of toughened polyimide materials for use in high-reliability multilayers. This combined resin system provides excellent thermal perform.. |
|||
Dielectric Breakdown | >= 50000 V | >= 50000 V | IPC-TM-650.2.5.6 |
Park Electrochemical Nelco® N7000-2 V0 Toughened Polyimide Laminate and Prepreg The Nelco N7000-2 V0 series is a next-generation high-Tg polyimide using a toughened resin chemistry to achieve a UL 94-V0 designation. This advanced material is designed for use in a wide variety o.. |
|||
Dielectric Breakdown | 50000 V | 50000 V | |
X Phenolic Laminate Paper based phenolic provides low cost electrical and mechanical properties. It is widely used for switchboards, panel boards, insulating washers, and intricate punched parts.Information provided b.. |
|||
Dielectric Breakdown | 50000 V @Thickness 1.57 mm |
50000 V @Thickness 0.0620 in |
Cond A; ASTM D229 S/S |
Industrial Laminates/Norplex NP320U Cotton Fabric Description: Utility version of NP320E. Meets most, but not all, NEMA properties for L and LE, and is not certifiable as a NEMA Grade.Thickness Tested: 0.062", 0.125", and 0.500" |
|||
Dielectric Breakdown | 50000 V @Thickness 1.57 mm |
50000 V @Thickness 0.0620 in |
Cond A; ASTM D229 S/S |
Industrial Laminates/Norplex NP639 Paper Base Laminate Description: Economical paper reinforced laminate developed with capacity to withstand temperatures to 150° C without blistering. High compressive strength and low moisture absorption.Thickness T.. |
|||
Dielectric Breakdown | 50000 V @Thickness 1.57 mm |
50000 V @Thickness 0.0620 in |
Cond A; ASTM D229 S/S |
Industrial Laminates/Norplex NP310U Cotton Fabric Description: Utility grade canvas phenolic with properties similar to NP310E.Not certifiable to NEMA due to low crosswise flexural strength. Previously designated NP310C.Thickness Tested: 0.062", 0... |
|||
Dielectric Breakdown | 50000 V | 50000 V | |
ExxonMobil Synesstic™ 12 Synthetic Fluid Product Description: Synesstic™ Alkylated Naphthalene (AN) represent a unique class of API Group V category fluids. Synesstic™ AN products offer improved hydrolytic, thermal and oxidative stabilit.. |
|||
Dielectric Breakdown | >= 50000 V | >= 50000 V | IPC-TM-650.2.5.6 |
Park Electrochemical Nelco® N4000-29 Multifunctional Epoxy The Nelco N4000-29 is an advanced, lead-free, low-CTE, high Tg (185º C by DSC) multifunctional epoxy dielectric substrate. This material has been designed for use not only in standard multilayer PW.. |
|||
Dielectric Breakdown | >= 50000 V | >= 50000 V | IPC-TM-650.2.5.6 |
Park Electrochemical Nelco® N4000-11 Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-11 is a CAF resistant, high Tg (175º C by DSC) multifunctional epoxy dielectric substrate. This material is formulated to provide the PWB manufacturer and OEM with vastly improved.. |