Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 60000 V | 60000 V | |
XX Phenolic Laminate Paper based phenolic provides low cost electrical and mechanical properties. It is widely used for switchboards, panel boards, insulating washers, and intricate punched parts.Information provided b.. |
|||
Dielectric Breakdown | 60000 V @Thickness 1.57 mm |
60000 V @Thickness 0.0620 in |
Cond A; ASTM D229 S/S |
Industrial Laminates/Norplex NP605 Paper Base Laminate Description: A paper-base laminate with low phenolic resin content for hard, flat surfaces. This material is normally used in the printed circuit board industry as a backup for the drilling operatio.. |
|||
Dielectric Breakdown | 60000 V | 60000 V | Parallel, Step-By-Step in Oil; ASTM D149 |
Haysite EMD Polyester, Glass Reinforced EMD is a glass mat reinforced polyester sheet designed primarily as a "slot wedge" material in large motors and generators. EMD has low weight loss at elevated temperatures and high flexural and sh.. |
|||
Dielectric Breakdown | >= 60000 V @Temperature 90.0 °C |
>= 60000 V @Temperature 194 °F |
Cond., In oil, Parallel to laminations; IEC 1212-2 6.2 |
Hippe PF CP 202 Cellulose Paper Reinforced Phenolic Resin - Sheet High voltage applications at power frequencies. High electric strength under oil. Good electrical strength in air under normal humidity.Information provided by Hippe. |
|||
Dielectric Breakdown | 60000 V | 60000 V | VDE Electrodes at 60 hertz (0.08 inch gap) |
ConocoPhillips Transformer Oil Description: Conoco Transformer Oil, an insulating oil of very high dielectric strength, is suited for oil-filled transformers in both large substations and small pole-mounted transformers. It is al.. |