Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 65000 V | 65000 V | |
XXX Phenolic Laminate Paper based phenolic provides low cost electrical and mechanical properties. It is widely used for switchboards, panel boards, insulating washers, and intricate punched parts.Information provided b.. |
|||
Dielectric Breakdown | 65000 V | 65000 V | |
Industrial Laminates/Norplex MC511A Glass Fabric Description: MC511A is a high strength, glass epoxy laminate that is specially formulated to meet power generation producer's exacting standards where higher strength at elevated temperatures ar.. |
|||
Dielectric Breakdown | 65000 V | 65000 V | IPC TM-650 2.5.6 |
Arlon EP2 Enhanced Polyimide Laminate and Prepreg High reliability and high temperature materialEP2 Enhanced Polyimide is the next generation of polyimide and prepreg products, engineered for improved properties and processing and for applications .. |