Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistivity | 747 - 747 Megaohm/1000 m @Temperature 15.6 - 15.6 °C |
2450 - 2450 Megaohm/1000 ft @Temperature 60.0 - 60.0 °F |
Average value: 747 Megaohm/1000 m Grade Count:1 |
Overview of materials for PVC, Wire and Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr.. |