Electrical Properties Metric English Comments
Insulation Resistivity 747 - 747 Megaohm/1000 m

@Temperature 15.6 - 15.6 °C
2450 - 2450 Megaohm/1000 ft

@Temperature 60.0 - 60.0 °F
Average value: 747 Megaohm/1000 m Grade Count:1
Overview of materials for PVC, Wire and Cable Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr..