Electrical Properties Metric English Comments
Curie Temperature 15.0 - 50.0 °C
59.0 - 122 °F
Special Metals DURANICKEL® 301 (UNS N03301) Annealed Rod and Bar
Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Annealed Rod and Bar specifically. Other property values are typical of ann..
Curie Temperature 15.0 - 50.0 °C
59.0 - 122 °F
Special Metals DURANICKEL® 301 (UNS N03301) Annealed Strip
Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Annealed Strip specifically. Other property values are typical of annealed DURANICKEL® alloy 3..
Curie Temperature 15.0 - 50.0 °C
59.0 - 122 °F
Special Metals DURANICKEL® 301 (UNS N03301) Annealed Wire
Tensile strength (ultimate) and elongation values reported here are typical for Annealed Wire specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the alloy in gen..
Curie Temperature 15.0 - 50.0 °C
59.0 - 122 °F
Special Metals DURANICKEL® 301 (UNS N03301) Cold-Drawn Rod and Bar
Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Cold-Drawn Rod and Bar specifically. Other property values are typical of annealed DURANICKEL®..
Curie Temperature 15.0 - 50.0 °C
59.0 - 122 °F
Special Metals DURANICKEL® 301 (UNS N03301) Half-Hard Strip
Tensile strength (ultimate), hardness, and elongation values reported here are typical for Half-Hard Strip specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the..
Curie Temperature 15.0 - 50.0 °C
59.0 - 122 °F
Special Metals DURANICKEL® 301 (UNS N03301) Hot-Finished Rod and Bar
Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Hot-Finished Rod and Bar specifically. Other property values are typical of annealed DURANICKELÂ..
Curie Temperature 15.0 - 50.0 °C
59.0 - 122 °F
Special Metals DURANICKEL® 301 (UNS N03301) Spring Strip
Tensile strength (ultimate), hardness, and elongation values reported here are typical for Spring Strip specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the al..
Curie Temperature 15.0 - 50.0 °C
59.0 - 122 °F
Special Metals DURANICKEL® 301 (UNS N03301) Spring Wire
Tensile strength (ultimate) and elongation values reported here are typical for Spring Wire specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the alloy in gener..
Curie Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Special Metals MONEL® Alloy 400
A nickel-copper alloy with high strength and excellent corrosion resistance in a range of media including sea water, hydrofluoric acid, sulfuric acid, and alkalis. Used for marine engineering, chem..
Curie Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Special Metals MONEL® Alloy R-405
The free-machining version of MONEL alloy 400. A controlled amount of sulfur is added to the alloy to provide sulfide inclusions that act as chip breakers during machining. Other characteristics a..