Electrical Properties Metric English Comments
Curie Temperature 460 °C
860 °F
Carpenter HyMu "80"® Electronic Alloy, Cold Rolled Strip
Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu..
Curie Temperature 460 °C
860 °F
Carpenter HyMu "80"® Electronic Alloy, Bar, After Process Anneal
Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu..
Curie Temperature 460 °C
860 °F
Carpenter HyMu "80"® Electronic Alloy, Cold Drawn Bar
Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu..
Curie Temperature 460 °C
860 °F
Carpenter HyMu "80"® Electronic Alloy, Hydrogen Annealed Bar
Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu..
Curie Temperature 460 °C
860 °F
Carpenter HyMu "80"® Electronic Alloy, Hydrogen Annealed Strip
Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu..
Curie Temperature 460 °C
860 °F
Carpenter HyMu "80"® Electronic Alloy, Strip, After Process Anneal
Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu..