Carpenter HyMu "80"® Electronic Alloy, Cold Rolled Strip

Category Metal , Electronic/Magnetic Alloy , Nonferrous Metal , Nickel Alloy
Manufacturer Carpenter Technology Corporation (Cartech)
Trade Name HyMu "80"®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Carpenter HyMu "80"® Electronic Alloy, Cold Rolled Strip.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximum permeability with minimum hysteresis loss.Carpenter HyMu “80” alloy has been used primarily in transformer cores, tape wound toroids and laminations where compactness and weight factors are important. It has also been used for shielding to protect electrical components from stray magnetic fields.HyMu "80"® is a registered trademark of Carpenter Technology Corporation.
Physical Properties Metric English Comments
Density 8.74 g/cc
0.316 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 100
100
Tensile Strength, Ultimate 930 MPa
135000 psi
Elongation at Break 4.0 %
4.0 %
Modulus of Elasticity 232 GPa
33600 ksi
Bar
Izod Impact 163 J
120 ft-lb
Bar
Thermal Properties Metric English Comments
CTE, linear 12.0 µm/m-°C

@Temperature 25.0 - 300 °C
6.67 µin/in-°F

@Temperature 77.0 - 572 °F
12.3 µm/m-°C

@Temperature 25.0 - 50.0 °C
6.83 µin/in-°F

@Temperature 77.0 - 122 °F
Specific Heat Capacity 0.494 J/g-°C
0.118 BTU/lb-°F
Thermal Conductivity 34.6 W/m-K
240 BTU-in/hr-ft²-°F
Melting Point 1454 °C
2649 °F
Solidus 1454 °C
2649 °F
Melting Point
Liquidus 1454 °C
2649 °F
Melting Point
Component Elements Properties Metric English Comments
Carbon, C 0.020 %
0.020 %
Iron, Fe 15 %
15 %
as remainder
Manganese, Mn 0.50 %
0.50 %
Molybdenum, Mo 4.2 %
4.2 %
Nickel, Ni 80 %
80 %
Silicon, Si 0.35 %
0.35 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000580 ohm-cm
0.0000580 ohm-cm
Temp Coefficient 0.0011/ºC (-17.8-449ºC)
Curie Temperature 460 °C
860 °F