Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | PLC code 4; UL 746A |
SABIC Innovative Plastics Cycolac® X17 ABS Automotive: Very high heat resistance with high strength and modulus. UL94 HB rated.This data was supplied by SABIC-IP for the Americas region. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Lexan® 103 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV stabilized for outdoor and lighting. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Lexan® 103 PC (Asia Pacific) Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV stabilized for outdoor and lighting. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Lexan® 123R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. Internal mold release. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Lexan® 203R PC 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Lexan® 203RM PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Lexan® 500ECR PC (Europe-Africa-Middle East) Lexan* 500ECR Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. It is of non-chlorinated & non-brominated flame retardant systems with UL-94 V0 rating at 2.3mm. It is a.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Lexan® LS2 PC (Asia Pacific) Automotive lens applications. Medium viscosity. UV-stabilized. Transparent colors only. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Lexan® LS3 PC (Asia Pacific) Automotive lens applications. Medium-high viscosity. UV-stabilized. Adhesion to coatings. Transparent colors only. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | PLC code 4; UL 746A |
SABIC Innovative Plastics Lexan® VR2020 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. Internal mold release.This data was supplied by SABIC-.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Cycolac® EX58 ABS (Europe-Africa-Middle East) High impact ABS for sheet extrusion and blow molding applications. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Cycolac® EX58F ABS (Asia Pacific) High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Lexan® 143 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 10.5 MFR. UV-stabilized. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Lexan® 143R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 10.5 MFR. UV-stabilized. Internal mold release. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | PLC code 4; UL 746A |
SABIC Innovative Plastics Lexan® 151 PC (Asia Pacific) Nonhalogenated. 2.5 MFR. Blowmolding/extrusion.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Lexan® 243 PC (Asia Pacific) 10.5 MFR. UV-stabilized. Improved flame retardance. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=0.750 mm |
7.0 - 15 sec @Thickness >=0.0295 in |
|
LG Chemical LUMID GP3150A(W) PA6+MF15%, General Purpose Feature: Injection Molding, PA6+MF15%, General PurposeApplication: E&E (Rice Cooer Housing)CAS No. 25038-54-4 and 14807-96-6Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | |
LG Chemical 95HCTC SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Lighter, Cosmetic Container, ToothbrushCAS No. 9003-54-7Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2310EPR PEI 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2310EPR PEI (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2312EPR PEI (Asia Pacific) 30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | PLC code 4; UL 746A |
SABIC Innovative Plastics Ultem 2412EPR PEI 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Am.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | PLC code 4; UL 746A |
SABIC Innovative Plastics Ultem 2412EPR PEI (Europe-Africa-Middle East) 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics NORYL GFN2 PPE+PS PPE+PS blend. 20% Glass reinforced. UL746C F1. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional sta.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Valox® V3504 PBT (Asia Pacific) VALOX EXVX0197 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics NORYL GFN3 PPE+PS PPE+PS blend. 30% Glass reinforced. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Sui.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 0.750 mm |
7.0 - 15 sec @Thickness 0.0295 in |
PLC 4 |
Eurostar Starflam P10002E PA6, Injection Molded Starflam P10002E is a Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding Resin (also known as P1000Z220 or PA6 U2 Z22)Information provided by Polymer Tec.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | |
DuPont Teijin Films Mylar® EL21 Polyester Film, 900 Gauge Mylar® EL21 polyester films are flexible strong and durable films with an unusual balance of properties, making them suitable for a variety of industrial applications. The excellent dielectric stre.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Lexan® 103R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV Stabilized for outdoor and lighting. Internal mold release... |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=0.750 mm |
7.0 - 15 sec @Thickness >=0.0295 in |
|
LG Chemical LUMID GP3300A(W) PA6+MF30%, General Purpose Feature: Injection Molding, PA6+MF30%, General PurposeApplication: Automotive (Battery Pack Housing)Information provided by LG Chemical |