Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Cycolac® EXABS01 ABS Sheet extrusion ABS with medium impact. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | PLC code 4; UL 746A |
SABIC Innovative Plastics Cycolac® X15 ABS Automotive. Very high heat resistance with high impact. UL94 HB rated. High gloss.This data was supplied by SABIC-IP for the Americas region. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Lexan® 123R PC (Asia Pacific) Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. Internal mold release. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Lexan® 203 PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Lexan® 203RM PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | PLC code 4; UL 746A |
SABIC Innovative Plastics Lexan® 223 PC 17.5 MFR, for small, intricate parts. Improved flame retardance. UV stabilized.This data was supplied by SABIC-IP for the Americas region. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Lexan® 223R PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Lexan® 500ECR PC (Europe-Africa-Middle East) Lexan* 500ECR Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. It is of non-chlorinated & non-brominated flame retardant systems with UL-94 V0 rating at 2.3mm. It is a.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Lexan® LS2 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Automotive lens applications. Medium viscosity. UV-stabilized. Transparent colors only. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Cycolac® EX58 ABS (Europe-Africa-Middle East) High impact ABS for sheet extrusion and blow molding applications. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Cycolac® EX58F ABS High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Cycolac® EX58F ABS (Asia Pacific) High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Lexan® 143 PC (Asia Pacific) Nonhalogenated. 10.5 MFR. UV-stabilized. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Lexan® 243 PC (Asia Pacific) 10.5 MFR. UV-stabilized. Improved flame retardance. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=0.750 mm |
7.0 - 15 sec @Thickness >=0.0295 in |
|
LG Chemical LUMID GP3150A(W) PA6+MF15%, General Purpose Feature: Injection Molding, PA6+MF15%, General PurposeApplication: E&E (Rice Cooer Housing)CAS No. 25038-54-4 and 14807-96-6Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | PLC code 4; UL 746A |
SABIC Innovative Plastics Ultem 2312EPR PEI (Europe-Africa-Middle East) 30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | PLC code 4; UL 746A |
SABIC Innovative Plastics Ultem 2412EPR PEI 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Am.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Valox® ENH3500 PBT (Europe-Africa-Middle East) Unfilled PBT, Non-Brominated & Non-Chlorinated Flame Retardant |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | |
DuPont Teijin Films Mylar® A Polyester Film, 1000 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Hot Wire Ignition, HWI | <= 7.0 sec | <= 7.0 sec | |
DuPont Teijin Films Mylar® A Polyester Film, 142 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness 0.750 mm |
7.0 - 15 sec @Thickness 0.0295 in |
PLC 4 |
Eurostar Starflam P10002E PA6, Injection Molded Starflam P10002E is a Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding Resin (also known as P1000Z220 or PA6 U2 Z22)Information provided by Polymer Tec.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | |
DuPont Teijin Films Mylar® EL21 Polyester Film, 750 Gauge Mylar® EL21 polyester films are flexible strong and durable films with an unusual balance of properties, making them suitable for a variety of industrial applications. The excellent dielectric stre.. |
|||
Hot Wire Ignition, HWI | <= 7.0 sec | <= 7.0 sec | |
DuPont Teijin Films Mylar® LBTW Polyester Film, 75 Gauge Mylar® LBTW is an uncoated, transparent polyester film that has been corona treated on one side to provide superior wetting and adhesion of inks, primers, and adhesives. Mylar® LBTW is commerciall.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | |
DuPont Teijin Films Mylar® MO21 Polyester Film, 1000 Gauge Product Description: Mylar® type MO21 films are strong, heavy gauge films that have excellent electrical properties. These films offer exceptional cut-through resistance, low shrinkage, low moistur.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | |
DuPont Teijin Films Mylar® MO21 Polyester Film, 900 Gauge Product Description: Mylar® type MO21 films are strong, heavy gauge films that have excellent electrical properties. These films offer exceptional cut-through resistance, low shrinkage, low moistur.. |
|||
Hot Wire Ignition, HWI | <= 7.0 sec | <= 7.0 sec | |
DuPont Teijin Films Mylar® A Polyester Film, 400 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Hot Wire Ignition, HWI | <= 7.0 sec | <= 7.0 sec | |
DuPont Teijin Films Mylar® A Polyester Film, 500 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | |
DuPont Teijin Films Mylar® A Polyester Film, 900 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Hot Wire Ignition, HWI | <= 7.0 sec | <= 7.0 sec | |
DuPont Teijin Films Mylar® A Polyester Film, 92 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Lexan® 103R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV Stabilized for outdoor and lighting. Internal mold release... |