Electrical Properties Metric English Comments
High Voltage Arc-Tracking Rate, HVTR 4.20 mm/min
0.165 in/min
UL 746A
Solvay Specialty Polymers Amodel® AT-5001 Polyphthalamide (PPA) Resin, Dry as Molded  (discontinued **)
AMODEL AT-5001 polyphthalamide resin is a neat ductile material that offers superior retention of properties after humid thermal aging, high impact at low temperature, and better mechanical properti..