Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 1.77 kV/mm | 45.0 kV/in | ASTM D495 |
Zircar Refractory Composites ZIRCAL-45 Refractory Board Type ZIRCAL-45 Refractory Board is a self supporting, high strength, rigid refractory product fabricated from calcium silicate, inert fillers and reinforcing agents. Its high structural strength com.. |
|||
Dielectric Strength | 1.77 kV/mm | 45.0 kV/in | ASTM D495 |
BNZ Materials Marinite® I&M High Temperature Structural Insulation Oven dried formulations of BNZ boards are used in a variety of heat insulating processes, fire protection and machined parts. Selection is commonly based on a balance between strength and insulating.. |
|||
Dielectric Strength | 1.77 kV/mm | 45.0 kV/in | |
Aremco Glass-Coat™ GC4000 High Temperature Specialty Coatings Glass Glass-enamel, gloss-black coating for stainless steel to 1000°F (538°C) |