Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 11.7 kV/mm | 297 kV/in | Step by Step; ASTM D149 |
Plenco 1530 Polyester, Briquette, Injection Molded PLENCO 01530 is a glass and mineral reinforced pelletized polyester molding compound, offering improved mechanical strength properties along with excellent electrical properties and dimensional stab.. |
|||
Dielectric Strength | 11.7 kV/mm | 297 kV/in | Short Time; ASTM D149 |
Plenco 6401 Phenolic, Briquette, Transfer Molded PLENCO 06401 is a glass fiber and mineral filled two-stage phenolic molding compound. UL recognized under component file E40654. 06401 is available in black.Information supplied by Plenco. |
|||
Dielectric Strength | 11.7 kV/mm | 297 kV/in | Step by Step; ASTM D149 |
Plenco 1506 Polyester, Briquette, Injection Molded PLENCO 01506 is a mineral and cellulose filled granular polyester molding compound, with glass fiber reinforcement for improved mechanical strength properties. 01506 offers excellent electrical prop.. |