Electrical Properties Metric English Comments
Dielectric Strength 47.0 kV/mm
1190 kV/in
IEC 243
LG Chemical RS-650 ABS, Extrusion, General Purpose
Information Provided by LG Chem
Dielectric Strength 47.0 kV/mm
1190 kV/in
Von Roll Isola IMI Varnish 271 Spirit Gum Varnish for Electrical Insulation
Data provided by Von Roll Isola USA.Flash Point:
Dielectric Strength 47.0 kV/mm
1190 kV/in
Full-wave Impulse; ASTM D3426
DuPont™ Nomex® 414 Paper, 15 mil Nominal Thickness
Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand..
Dielectric Strength 47.0 kV/mm
1190 kV/in
IEC 60243-1
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi..