Von Roll Isola IMI Varnish 271 Spirit Gum Varnish for Electrical Insulation

Category Polymer , Thermoset
Manufacturer Von Roll Isola
Trade Name IMI Varnish
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Von Roll Isola IMI Varnish 271 Spirit Gum Varnish for Electrical Insulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Von Roll Isola USA.Flash Point:
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
Viscosity 1500 cP
1500 cP
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
Electrical Properties Metric English Comments
Dielectric Strength 47.0 kV/mm
1190 kV/in
Processing Properties Metric English Comments
Processing Temperature 135 °C
275 °F
Suggested baking time at this temperature is 0.5-1 hr.