Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 51.0 kV/mm | 1300 kV/in | IEC 60243-1 |
PolyOne OnFlex™ AW 300-02 Thermoplastic Elastomer (TPE) OnFlex™ AW 300-02 is a non-halogen flame retardant material designed for appliance wire applications. New Product. Commercial specifications have not been established.Purge thoroughly before and af.. |
|||
Dielectric Strength | 51.0 kV/mm @Thickness 0.533 mm, Temperature 23.0 °C |
1300 kV/in @Thickness 0.0210 in, Temperature 73.4 °F |
50% RH, ASTM D149-97a(04); ASTM D149 |
PolyOne OnFlex™ HFFR 315-01 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 315-01 a is non-halogen flame retardant material designed for flexible power cord insulation, cable jackets, and ribbon cables. New Product. Commercial specifications have not been est.. |
|||
Dielectric Strength | 51.2 - 59.1 kV/mm | 1300 - 1500 kV/in | ASTM D149 |
Arkema Group Kynar Flex® 2900 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Dielectric Strength | 51.2 - 59.1 kV/mm | 1300 - 1500 kV/in | ASTM D149 |
Arkema Group Kynar Flex® 3120 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Dielectric Strength | 51.2 kV/mm | 1300 kV/in | |
Saint-Gobain CHR® SG03-06(R) Premium Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Dielectric Strength | 51.0 kV/mm | 1300 kV/in | Full-wave Impulse; ASTM D3426 |
DuPont™ Nomex® 414 Paper, 10 mil Nominal Thickness Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand.. |
|||
Dielectric Strength | 51.0 kV/mm | 1300 kV/in | Full-wave Impulse; ASTM D3426 |
DuPont™ Nomex® 414 Paper, 12 mil Nominal Thickness Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand.. |
|||
Dielectric Strength | 51.0 kV/mm | 1300 kV/in | Full-wave Impulse; ASTM D3426 |
DuPont™ Nomex® 414 Paper, 7 mil Nominal Thickness Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand.. |
|||
Dielectric Strength | 51.2 kV/mm | 1300 kV/in | ASTM D149 |
ExxonMobil LDPE LD 150BW Wire & Cable Low Density Polyethylene Resin Product Description: LD 150BW is a LDPE containing suitable for the production of LV and MV crosslinked insulation using the 1-step or 2-step silane technology. Through in-house compounding it can a.. |
|||
Dielectric Strength | 51.2 kV/mm | 1300 kV/in | ASTM D149 |
ExxonMobil LDPE LD 419.MV Low Density Polyethylene Resin Product Description: LD 419.MV is a LDPE designed for wire and cable applications and is suitable for making crosslinkable compounds for medium voltage insulation.Availability: Latin America, North .. |
|||
Dielectric Strength | 51.2 kV/mm | 1300 kV/in | ASTM D149 |
ExxonMobil LLDPE LL 1001XV Wire & Cable Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 1001 XV is a C4 Ziegler Natta LLDPE for power cable and Telecom jacketing. The grade contains a low level of antioxidants and has excellent Environmental Stress Crack Resista.. |
|||
Dielectric Strength | 51.2 kV/mm | 1300 kV/in | ASTM D149 |
ExxonMobil LLDPE LL 1004YB Wire & Cable Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 1004YB is a C4 Ziegler Natta LLDPE, especially designed for Low Voltage power cable insulation, using the two-step silane cross-linking process. The grade contains a higher l.. |
|||
Dielectric Strength | 51.2 kV/mm | 1300 kV/in | 12 to 14 mil coating; ASTM D149 |
3M Scotchcast™ 5555 10G Electrical Insulating Epoxy Resin 3M Scotchcast Electrical Resin 5555 is a one-part, green pigmented, rapid heat curing powder coating. It is designed to provide a continuous, tough moisture and chemical resistant dielectric coating.. |
|||
Dielectric Strength | 51.2 kV/mm | 1300 kV/in | 12 to 14 mil coating; ASTM D149 |
3M Scotchcast™ 5555 22G Electrical Insulating Epoxy Resin 3M Scotchcast Electrical Resin 5555 is a one-part, green pigmented, rapid heat curing powder coating. It is designed to provide a continuous, tough moisture and chemical resistant dielectric coating.. |
|||
Dielectric Strength | 51.2 - 59.1 kV/mm | 1300 - 1500 kV/in | ASTM D149 |
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |
|||
Dielectric Strength | 51.2 - 59.1 kV/mm | 1300 - 1500 kV/in | ASTM D149 |
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s.. |
|||
Dielectric Strength | 51.2 - 63.0 kV/mm | 1300 - 1600 kV/in | ASTM D149 |
Arkema Group KYNAR FLEX® 2850 Black Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Dielectric Strength | 51.2 - 63.0 kV/mm | 1300 - 1600 kV/in | ASTM D149 |
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Dielectric Strength | 51.2 - 63.0 kV/mm | 1300 - 1600 kV/in | ASTM D149 |
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Dielectric Strength | 51.2 - 59.1 kV/mm | 1300 - 1500 kV/in | ASTM D149 |
Arkema Group KYNAR FLEX® 2900-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness.. |
|||
Dielectric Strength | 51.2 - 59.1 kV/mm | 1300 - 1500 kV/in | ASTM D149 |
Arkema Group KYNAR FLEX® 3120-15 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness.. |
|||
Dielectric Strength | 51.2 - 59.1 kV/mm | 1300 - 1500 kV/in | ASTM D149 |
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Dielectric Strength | 51.2 kV/mm | 1300 kV/in | |
3M 92015 Double Coated Tape with Adhesive 200MP 3M™ Double Coated Tapes with 3M™ Adhesive 200MP feature a thin polyester film for dimensional stability and improved handling with ease of die-cutting and laminating. The 3M adhesive 200MP provide.. |
|||
Dielectric Strength | 51.2 kV/mm | 1300 kV/in | 12 to 15 mil coating; ASTM D149 |
3M Scotchcast™ 265 Electrical Epoxy Powder Resin 3M Scotchcast Electrical Resin 265 is a new solution to an old problem. Historically, manufactures of coils, stators and armatures have used liquid-based varnishes or resins to coat and impregnate t.. |
|||
Dielectric Strength | 51.2 kV/mm | 1300 kV/in | IPC-TM-650.2.5.6.2 |
Park Electrochemical Nelco® N4000-11 BC® Buried Capacitance™ Epoxy Laminate and Prepreg The Nelco® N4000-11 is a CAF resistant, high Tg (175º C by DSC) multifunctional epoxy dielectric substrate. This material is formulated to provide the PWB manufacturer and OEM with vastly improved.. |
|||
Dielectric Strength | 51.2 kV/mm | 1300 kV/in | ASTM D1000 |
Saint-Gobain Furon®, Kapton® K275 Tape Description: A 1 mil thermally conductive Kapton® film, coated on both sides with 2 mils of thermally-conductive pressure-sensitive adhesive. Recommended uses: Excellent for use in small, compact e.. |
|||
Dielectric Strength | 51.2 kV/mm | 1300 kV/in | IPC-TM-650.2.5.6.2 |
Park Electrochemical Nelco® N4000-11 Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-11 is a CAF resistant, high Tg (175º C by DSC) multifunctional epoxy dielectric substrate. This material is formulated to provide the PWB manufacturer and OEM with vastly improved.. |
|||
Dielectric Strength | 51.2 - 59.1 kV/mm | 1300 - 1500 kV/in | ASTM D149 |
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |
|||
Dielectric Strength | 51.2 - 63.0 kV/mm | 1300 - 1600 kV/in | ASTM D149 |
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Dielectric Strength | 51.2 - 63.0 kV/mm | 1300 - 1600 kV/in | ASTM D149 |
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |