Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 51.0 kV/mm | 1300 kV/in | IEC 60243-1 |
PolyOne OnFlex™ AW 300-02 Thermoplastic Elastomer (TPE) OnFlex™ AW 300-02 is a non-halogen flame retardant material designed for appliance wire applications. New Product. Commercial specifications have not been established.Purge thoroughly before and af.. |
|||
Dielectric Strength | 51.0 kV/mm @Thickness 0.533 mm, Temperature 23.0 °C |
1300 kV/in @Thickness 0.0210 in, Temperature 73.4 °F |
50% RH, ASTM D149-97a(04); ASTM D149 |
PolyOne OnFlex™ HFFR 315-01 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 315-01 a is non-halogen flame retardant material designed for flexible power cord insulation, cable jackets, and ribbon cables. New Product. Commercial specifications have not been est.. |
|||
Dielectric Strength | 51.0 kV/mm | 1300 kV/in | Full-wave Impulse; ASTM D3426 |
DuPont™ Nomex® 414 Paper, 10 mil Nominal Thickness Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand.. |
|||
Dielectric Strength | 51.0 kV/mm | 1300 kV/in | Full-wave Impulse; ASTM D3426 |
DuPont™ Nomex® 414 Paper, 12 mil Nominal Thickness Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand.. |
|||
Dielectric Strength | 51.0 kV/mm | 1300 kV/in | Full-wave Impulse; ASTM D3426 |
DuPont™ Nomex® 414 Paper, 7 mil Nominal Thickness Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand.. |