Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dielectric Strength = 15.2 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 15.2 kV/mm
385 kV/in
Short Term; ASTM D149
Quadrant EPP Ertalyte® PET-P, Polyester-semi-crystalline thermoplastic, extruded (ASTM Product Data Sheet)
Dielectric Strength 15.2 kV/mm
385 kV/in
Short Term; ASTM D149
Quadrant EPP Techtron® PSGF PPS - Compression Molded 40% Glass Reinforced Polyphenylene Sulfide (ASTM Product Data Sheet)
Dielectric Strength 15.2 kV/mm
385 kV/in
ASTM D149
Technetics Group Amicon™ PET-P  (Unverified Data**)
Information provided by Technetics Group (formerly Plastomer Technologies)
Dielectric Strength >= 15.2 kV/mm

@Temperature 121 °C,
Time 10800 sec
>= 385 kV/in

@Temperature 250 °F,
Time 3.00 hour
0.0625 in. thickness; ASTM D149
Garlock MULTI-SWELLâ„¢ 3760 Compressed Aramid Fiber Gasketing
Aramid fibers with a proprietary rubber binder.Creates compressive load in light weight flanges in oil and water serviceTwice as compressible as standard fiber gasketsSeals with low load and irregul..
Dielectric Strength 15.2 kV/mm
386 kV/in
60Hz, Step-by-Step, dry; ASTM D149
Sumitomo Bakelite North America E 8353-706R-1 Hardware Grade Epoxy
Fiberglass and mineral reinforced epoxy molding compound with excellent dimensional stability and good strength at elevated temperatures.Information provided by Vyncolit, a Sumitomo Bak Group
Dielectric Strength 15.2 kV/mm
386 kV/in
Short Time; ASTM D149
Plenco 6990 Phenolic, Briquette, Compression Molded
PLENCO 06990 is a glass and mineral filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco.
Dielectric Strength 15.2 kV/mm
385 kV/in
Tra-Con Tra-Cast 3010 Flexible Clear Epoxy Casting Compound
TRA-CAST 3010 is a clear, low viscosity epoxy casting compound recommended for industrial embedding and casting applications where its combination of superior properties, good clarity, long pot life..
Dielectric Strength 15.2 kV/mm
385 kV/in
Dow Corning SLYGARD® 527 A&B SILICONE DIELECTRIC GEL
Two-parts, clear, RT or heat cure.Information provided by Dow Corning
Dielectric Strength 15.2 kV/mm
385 kV/in
ASTM D149
DSM Biomedical Elasthane™ 55D Thermoplastic Polyether Polyurethane (TPU)
A high tensile strength, aromatic biomedical polymer with an exceptional combination of mechanical properties plus biological compatibility Elasthane™ TPU exhibits outstanding hydrolytic stabilit..
Dielectric Strength 15.2 kV/mm
385 kV/in
Dow Corning 3-4150 DIELECTRIC GEL KIT
Two-part, transparent green, fast RT or heat cure.Information provided by Dow Corning
Dielectric Strength 15.2 - 16.9 kV/mm
385 - 430 kV/in
Short Time
Bulk Molding Compounds BMC 8005 Polyester Molding Compound
Dielectric Strength 15.2 - 16.7 kV/mm
386 - 424 kV/in
DC Breakdown Strength
China-Yixing Longly Refractories 99 Alumina Ceramic Tubes & Rods
LONGLY's alumina ceramic tubes and rods (the tolerances of +/- 0.02mm could be reached by mechanical or electronic finishing or mirror surface finishing) have high hardness, wear resistance, insulat..