Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 16.4 kV/mm @Thickness 2.00 mm |
417 kV/in @Thickness 0.0787 in |
IEC 60243-1 |
Gromax 1140LH TPE Product Description: 1140LH is Low modulus grade with nominal Durometer hardness of 40D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like inject.. |
|||
Dielectric Strength | 16.4 kV/mm | 417 kV/in | 60Hz, Short Time, dry; ASTM D149 |
Sumitomo Bakelite North America E 3938A Hardware Grade Epoxy Fiberglass reinforced epoxy molding compound with excellent dimensional stability, good strength and excellent electrical insulation properties.Information provided by Vyncolit, a Sumitomo Bak Group.. |
|||
Dielectric Strength | 16.4 kV/mm | 417 kV/in | 60Hz, Short Time, wet; ASTM D149 |
Sumitomo Bakelite North America E 8353-706R-1 Hardware Grade Epoxy Fiberglass and mineral reinforced epoxy molding compound with excellent dimensional stability and good strength at elevated temperatures.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Dielectric Strength | 16.4 kV/mm | 416 kV/in | |
Dow Corning HV 1650/50 SILICONE RUBBER 50 Shore A hardness high consistency silicone rubber with excellent tracking and erosion resistance and low modulusInformation provided by Dow Corning |
|||
Dielectric Strength | 16.4 kV/mm | 417 kV/in | Short Time; ASTM D149 |
Plenco 51030 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 51030 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for good physical strength. It is UL listed.Information supplied by PlencoPlenco discontinued.. |