Polymer Property : Dielectric Strength = 2.40 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 2.40 kV/mm

@Thickness 1.59 mm
61.0 kV/in

@Thickness 0.0625 in
100% RH for 96 hours; ASTM D149
Garlock GYLON® 3500 PTFE Gasketing, Silica Filler
PTFE with silica filler.Improved sealing performance over conventional PTFEUnique manufacturing process minimizes cold flow problems typical of skived and expanded PTFE sheetsExcellent bolt torque r..
Dielectric Strength 2.40 kV/mm
61.0 kV/in
ASTM D495
Zircar Refractory Composites ZIRCAL-95 Refractory Board
Type ZIRCAL-95 Refractory Board is produced from a combination of natural organic fibers and inert reinforcing fillers in a high density calcium silicate hydrate matrix. Designed as a substitute for..
Dielectric Strength 2.40 kV/mm

@Diameter >=3.00 mm
61.0 kV/in

@Diameter >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60243-1; IEC/EN 61212-2 6.1.2.1
Elektro-Isola G-Etronax EP 10 Epoxy, Glass Fabric Reinforcement, Light Yellow, Tubes
Description: Particularly good electrical and mechanical properties. Extremely high mechanical strength. Retains electrical properties at high air humidity. High resistance to chemicals.Applications..
Dielectric Strength 2.40 kV/mm

@Diameter >=3.00 mm
61.0 kV/in

@Diameter >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60243-1; IEC/EN 61212-2 6.1.2.1
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Tubes
Description: Particularly good electrical and mechanical properties. Extremely high mechanical strength, even at high temperatures. Retains electrical properties at high air humidity. High resistanc..
Dielectric Strength 2.40 kV/mm

@Diameter >=3.00 mm
61.0 kV/in

@Diameter >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60243-1; IEC/EN 61212-2 6.1.2.1
Elektro-Isola G-Etronax EP 22 Epoxy, Glass Fabric Reinforcement, Light Yellow, Tubes
Description: Particularly good electrical and mechanical properties. Extremely high mechanical strength, even at high temperatures. Retains electrical properties at high air humidity. High resistanc..
Dielectric Strength 2.40 kV/mm
61.0 kV/in
ASTM D495
BNZ Materials CS85 High Temperature Structural Insulation
NZ manufactures a variety of non-asbestos calcium silicate structural insulations that combine high strength and excellent thermal insulating characteristics for use in a variety of heat processing,..