Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 2.40 kV/mm @Thickness 1.59 mm |
61.0 kV/in @Thickness 0.0625 in |
100% RH for 96 hours; ASTM D149 |
Garlock GYLON® 3500 PTFE Gasketing, Silica Filler PTFE with silica filler.Improved sealing performance over conventional PTFEUnique manufacturing process minimizes cold flow problems typical of skived and expanded PTFE sheetsExcellent bolt torque r.. |
|||
Dielectric Strength | 2.40 kV/mm | 61.0 kV/in | ASTM D495 |
Zircar Refractory Composites ZIRCAL-95 Refractory Board Type ZIRCAL-95 Refractory Board is produced from a combination of natural organic fibers and inert reinforcing fillers in a high density calcium silicate hydrate matrix. Designed as a substitute for.. |
|||
Dielectric Strength | 2.40 kV/mm @Diameter >=3.00 mm |
61.0 kV/in @Diameter >=0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60243-1; IEC/EN 61212-2 6.1.2.1 |
Elektro-Isola G-Etronax EP 10 Epoxy, Glass Fabric Reinforcement, Light Yellow, Tubes Description: Particularly good electrical and mechanical properties. Extremely high mechanical strength. Retains electrical properties at high air humidity. High resistance to chemicals.Applications.. |
|||
Dielectric Strength | 2.40 kV/mm @Diameter >=3.00 mm |
61.0 kV/in @Diameter >=0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60243-1; IEC/EN 61212-2 6.1.2.1 |
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Tubes Description: Particularly good electrical and mechanical properties. Extremely high mechanical strength, even at high temperatures. Retains electrical properties at high air humidity. High resistanc.. |
|||
Dielectric Strength | 2.40 kV/mm @Diameter >=3.00 mm |
61.0 kV/in @Diameter >=0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60243-1; IEC/EN 61212-2 6.1.2.1 |
Elektro-Isola G-Etronax EP 22 Epoxy, Glass Fabric Reinforcement, Light Yellow, Tubes Description: Particularly good electrical and mechanical properties. Extremely high mechanical strength, even at high temperatures. Retains electrical properties at high air humidity. High resistanc.. |
|||
Dielectric Strength | 2.40 kV/mm | 61.0 kV/in | ASTM D495 |
BNZ Materials CS85 High Temperature Structural Insulation NZ manufactures a variety of non-asbestos calcium silicate structural insulations that combine high strength and excellent thermal insulating characteristics for use in a variety of heat processing,.. |