Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 20.2 kV/mm @Thickness 3.20 mm |
513 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® 4501 PPC (Asia Pacific) High heat resistant polyphthlate carbonate, provides DTUL of 290F at 264 psi. |
|||
Dielectric Strength | 20.2 kV/mm @Thickness 3.20 mm |
513 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® 4504 PPC High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with .. |
|||
Dielectric Strength | 20.2 kV/mm @Thickness 3.20 mm |
513 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® 4504 PPC (Asia Pacific) High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit.. |
|||
Dielectric Strength | 20.2 kV/mm @Thickness 3.20 mm |
513 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Dielectric Strength | 20.2 kV/mm @Thickness 3.20 mm |
513 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Dielectric Strength | 20.2 kV/mm @Thickness 3.20 mm |
513 kV/in @Thickness 0.126 in |
in air; ASTM D 149 |
SABIC Innovative Plastics Lexan® HPH4504 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Dielectric Strength | 20.2 kV/mm @Thickness 3.20 mm |
513 kV/in @Thickness 0.126 in |
in air; ASTM D 149 |
SABIC Innovative Plastics Lexan® HPH4504H PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Dielectric Strength | 20.2 kV/mm @Thickness 3.20 mm |
513 kV/in @Thickness 0.126 in |
in air; ASTM D 149 |
SABIC Innovative Plastics Lexan® PPC4504 PPC High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit.. |
|||
Dielectric Strength | 20.2 kV/mm @Thickness 3.20 mm |
513 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® 4501 PPC High heat resistant polyphthlate carbonate, provides DTUL of 290F at 264 psi. |
|||
Dielectric Strength | 20.2 kV/mm @Thickness 3.20 mm |
513 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Dielectric Strength | 20.2 kV/mm @Thickness 3.20 mm |
513 kV/in @Thickness 0.126 in |
in air; ASTM D 149 |
SABIC Innovative Plastics Lexan® ML5472 PC Gamma sterilization resistant. High heat (PPC). Available in natural color only. Internal mold release.This data was supplied by SABIC-IP for the Americas region. |
|||
Dielectric Strength | 20.2 kV/mm | 513 kV/in | |
Covestro Desmopan® 588 Thermoplastic Polyurethane Desmopan 588 is a TPU on the basis of a special ether with good microbe-resistance.Applications: Cable sheathing, hoses, profiles.Information provided by Bayer.As of 1 September 2015, Bayer Material.. |
|||
Dielectric Strength | 20.2 kV/mm | 513 kV/in | ASTM D149 |
Arlon 55579XA028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production material an.. |
|||
Dielectric Strength | 20.2 kV/mm | 514 kV/in | ASTM D149 |
Arlon 49283R040 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil polyethylene; Side 1: cured silicone rubber; Substrate: 1681 Fiberglass; Side 2: cured silicone rubber |
|||
Dielectric Strength | 20.2 kV/mm | 513 kV/in | ASTM D149 |
Covestro Petlon® 3530 Semi-Crystalline PET, 30% Glass Fiber
(discontinued **) Characteristics: Excellent Electrical Properties, High Heat and Chemical ResistanceApplications: Automotive (Underhood), Appliances, Casings and HousingsProcessing: Injection Molding (Melt Temperatu.. |