Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 49283R040 Silicone Rubber/Fiberglass Laminate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 49283R040 Silicone Rubber/Fiberglass Laminate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Interleave: 3 mil polyethylene; Side 1: cured silicone rubber; Substrate: 1681 Fiberglass; Side 2: cured silicone rubber
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
silicone property; Arlon SQA-TMS-024
Thickness 140 microns
5.50 mil
substrate; Arlon SQA-TMS-003
419 microns
16.5 mil
side 1 silicone; Arlon SQA-TMS-003
457 microns
18.0 mil
side 2 silicone; Arlon SQA-TMS-003
1020 microns
40.0 mil
overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
silicone property; ASTM D2240
Tensile Strength, Ultimate 9.03 MPa
1310 psi
silicone property; ASTM D412
Elongation at Break 338 %
338 %
silicone property; ASTM D412
Tear Strength 20.9 kN/m
119 pli
silicone property; ASTM D624
Compression Set 49 %
49 %
Arlon SQA-TMS-017
Thermal Properties Metric English Comments
Thermal Conductivity 0.8467 W/m-K
5.876 BTU-in/hr-ft²-°F
Resistance of 1.2E-3 m²K/W; Arlon SQA-TMS-054
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 20.2 kV/mm
514 kV/in
ASTM D149
Processing Properties Metric English Comments
Shelf Life 60.0 Month

@Temperature 23.9 °C
60.0 Month

@Temperature 75.0 °F
Descriptive Properties Value Comments
Color Red
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved