Polymer Property : Dielectric Strength = 2160 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 15.0 - 85.0 kV/mm
380 - 2160 kV/in
Average value: 34.7 kV/mm Grade Count:21
Overview of materials for Nylon 66, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu..
Dielectric Strength 15.0 - 85.0 kV/mm
380 - 2160 kV/in
Average value: 29.9 kV/mm Grade Count:39
Overview of materials for Nylon 66, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu..
Dielectric Strength 25.0 - 85.0 kV/mm
635 - 2160 kV/in
DIN 53481
Isoflon PETP Polyethylene terephthalate
Good optical propertiesHigh UV resistanceAbsorbs little moistureInformation provided by Isoflon.