Electrical Properties Metric English Comments
Dielectric Strength 22.7 kV/mm
577 kV/in
ASTM D149
Covestro Petlon® 4630 Semi-Crystalline PET, 30% Glass Fiber  (discontinued **)
Characteristics: Flame Retardant: Electrical Properties, High Heat and Chemical ResistanceApplications: Connectors, Relays, Switches, Automotive (Under Hood), AppliancesProcessing: Injection Molding..
Dielectric Strength 22.7 - 31.0 kV/mm
577 - 787 kV/in
Average value: 27.3 kV/mm Grade Count:6
Overview of materials for Polyarylamide, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyarylamide, Glass Fiber Filled". Each property range of values reported is minimum and maximum values..
Dielectric Strength 22.7 kV/mm
577 kV/in
Breakdown Voltage; ASTM D149
UBE UPIMOL® SA101 Heat-Resistant Polyimide Shape
Description: UPIMOL® SA101 is an excellent heat-resistant polyimide shape, based on Biphenyl tetracarboxilic dianhydride(BPDA) originally developed by UBE. UPIMOL® SA101 has improved high durabili..
Dielectric Strength 22.7 kV/mm
577 kV/in
ASTM D149
Arlon LW301C##FR-P1 0.030" (0.762 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: 1 inch wide, 30 mil thick, Brown, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length..
Dielectric Strength 22.7 kV/mm
577 kV/in
ASTM D149
Arlon LW201C##FR-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: High Strength, 1 inch wide, 20 mil thick, Brown, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indica..
Dielectric Strength 22.7 kV/mm
577 kV/in
ASTM D149
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, DAM  (discontinued **)<
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..