Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 1.26 - 24.5 kV/mm | 32.0 - 622 kV/in | Average value: 7.07 kV/mm Grade Count:4 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |