Electrical Properties Metric English Comments
Dielectric Strength 1.26 kV/mm
32.0 kV/in
Quadrant EPP Ketron® CA30 LSG PEEK, Extruded 30% Carbon Fiber Reinforced Polyetherether Ketone (ASTM Product Data Sheet)
Dielectric Strength 1.26 kV/mm
32.0 kV/in
Short Term; ASTM D149
Quadrant EPP Ketron® CA30 PEEK, Extruded 30% Carbon Fiber Reinforced Polyetherether Ketone (ASTM Product Data Sheet)
Dielectric Strength 1.26 kV/mm
32.0 kV/in
ASTM D149
Quantum PEEK 30% Carbon Filled
Information provided by Quantum Advanced Engineering Plastics
Dielectric Strength 1.26 - 24.5 kV/mm
32.0 - 622 kV/in
Average value: 7.07 kV/mm Grade Count:4
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu..
Dielectric Strength 1.26 kV/mm
32.0 kV/in
ASTM D149
Technetics Group Amicon™ PEEK 30% Carbon  (Unverified Data**)
Information provided by Technetics Group (formerly Plastomer Technologies)