Electrical Properties Metric English Comments
Dielectric Strength 25.2 kV/mm
640 kV/in
ASTM D149
Polymer Resources PC-FR1A-D Polycarbonate, Flame Retardant, Low Flow
Polycarbonate, Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing co..
Dielectric Strength 25.2 kV/mm
640 kV/in
ASTM D149
Polymer Resources PC-FR2A-D Polycarbonate, Flame Retardant, Medium Flow
Polycarbonate, Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-i..
Dielectric Strength 25.2 kV/mm
640 kV/in
ASTM D149
Polymer Resources PC-FR2A-D-[color]-3 Polycarbonate, Flame Retardant, Medium Flow, UV-stabilized
Polycarbonate, Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
Dielectric Strength 25.2 kV/mm
640 kV/in
ASTM D149
Polymer Resources PC-FR3A-D Polycarbonate, Flame Retardant, High Flow
Polycarbonate, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by..
Dielectric Strength 25.2 kV/mm
640 kV/in
ASTM D149
Covestro Petlon® 8535 Semi-Crystalline PET, 35% Mineral/Glass Fiber  (discontinued **)
Characteristics: Impact Modified: Excellent Electrical Properties, High Heat ResistanceApplications: Automotive (Under Hood), Appliances, Casings and HousingsProcessing: Injection Molding (Melt Temp..
Dielectric Strength 25.2 kV/mm
640 kV/in
ASTM D149
Polymer Resources PC-FR1A-D-[color]-3 Polycarbonate, Flame Retardant, Low Flow, UV-stabilized
Polycarbonate, Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Dielectric Strength 25.2 kV/mm
640 kV/in
ASTM D149
Polymer Resources PC-FR3A-D-[color]-3 Polycarbonate, Flame Retardant, High Flow, UV-stabilized
Polycarbonate, Flame Retardant, High Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat..
Dielectric Strength 25.2 kV/mm
640 kV/in
Saint-Gobain CHR® 2915-7 Glass Cloth Backing Silicone Adhesive Pressure Sensitive Tape
Description: Glass cloth offers excellent abrasion resistance and mechanical properties, as well as high tensile strength and extreme temperature resistance. Service temperatures range from -100°..
Dielectric Strength 25.2 kV/mm
640 kV/in
ASTM D149
Plastics Group Polifil® 628L Nylon 6/6 (DAM)
Polifil® NYLON 6/6 combines good abrasion and chemical resistance.Applications: ValvesBearingsBearing casesStandard processing techniques are applicable. Information provided by The Plastics Group...
Dielectric Strength 25.2 kV/mm
640 kV/in
ASTM D149
Arlon 51576B015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave: Polyethylene This data represents typical values for the production mate..
Dielectric Strength 25.2 kV/mm
640 kV/in
ASTM D149
Arlon 55578R030 0.0325" (0.825 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneSide 1, Layer 2: Uncured Silicone Rubber Side 1, Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 2: Cured Silicone Rubber Appearance:..
Dielectric Strength 25.2 kV/mm
640 kV/in
ASTM D149
Arlon Thermabond® 48A43X008 0.008"(0.203 mm) Cured Silicone Rubber with Fiberglass Substrate
Description: Thermabond® Electrically insulating, thermally conductive, thermal interface material (TIM).Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1080 FiberglassSide 2: Cu..
Dielectric Strength 25.2 kV/mm
640 kV/in
ASTM D149
Arlon Thermabond® R37623X008 0.0050" Cured Silicone Rubber with Fiberglass Substrate
Thermabond®: Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction:Side 1: Cured Silicone RubberSubstrate: 1080-style FiberglassSide 2: Cured Silico..
Dielectric Strength 25.2 kV/mm
640 kV/in
ASTM D149
3M Scotch-Weld™ DP605NS Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-part, non-sag urethane adhesives. They feature tough, flexible bonds with good adhesion to a wide variety of substrates especially wood and many properl..
Dielectric Strength 25.2 kV/mm
640 kV/in
ASTM D149
Arlon 51576W015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: White silicone gum on glass fabricThis data re..
Dielectric Strength 25.2 kV/mm
640 kV/in
1" electrode in air; ASTM D149
Teknor Apex Sarlink® 4339D Thermoplastic Elastomer
A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4339D is a flame retardant, high hardness grade processing exceptional chemical resistance, compression set ..
Dielectric Strength 25.2 kV/mm
640 kV/in
ASTM D149
ExxonMobil Santoprene® 123-50 Thermoplastic Elastomer  (discontinued **)
A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran..