Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 268 kV/mm | 6800 kV/in | Short Time; 1 mil |
Parylene Coating Services C Poly (P-Xylylene) Monomer is monochloro para-xylylene. Parylene C is recommended where excellent barrier protection is needed. It can be used up to 125°C where oxygen is present.Parylene is a generic name for poly-.. |