Electrical Properties Metric English Comments
Dielectric Strength 30.5 kV/mm
775 kV/in
IEC 60243-1:1998-01
Global EPP PA 66E Extruded Polyamide 66
Polyamides, commonly referred to as nylons, are macromolecular, partially crystalline thermoplastics. Their physical properties are mainly determined by the composition and structure of their molecu..
Dielectric Strength 30.5 kV/mm
775 kV/in
IEC 60250
Polyram PlusTek PA201 Nylon 66 for Extrusion
High viscosity Nylon 66 for extrusion applications.Information provided by Polyram.
Dielectric Strength 30.5 kV/mm

@Thickness 0.400 mm
775 kV/in

@Thickness 0.0157 in
thick
Arkema Group Rilsan® Fine Powders Polyamide 11
Rilsan® fine powder coatings offer weatherability, long-lasting adhesion, chalk resistance, chemical resistance to aliphatic hydrocarbons, bases, salt solutions, oils, greases and other petroleum p..
Dielectric Strength 30.5 kV/mm
775 kV/in
ASTM D149
Arlon R36338R015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone Rubber Side 1, Layer 1: Uncured Silicone Rubber Substrate: Style 7628 FiberglassSide 2: Cured Silicone RubberAppearan..