Polymer Property : Dielectric Strength = 31.0 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 1.22 kV/mm

@Thickness 3.17 mm
31.0 kV/in

@Thickness 0.125 in
Unconditioned; ASTM D149
Garlock 19 SBR Rubber Gasketing, Cotton Reinforced
SBR rubber with cotton sheeting as fabric insertCombines elasticity and extensibility of rubber with strength of fabric insert. Specially compounded in varying burst strengths for almost any servic..