Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 60.0 - 339 kV/mm | 1520 - 8610 kV/in | Average value: 206 kV/mm Grade Count:56 |
Overview of materials for Polyimide, Thermoset Film This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Thermoset Film". Each property range of values reported is minimum and maximum values of appr.. |