Electrical Properties Metric English Comments
Dielectric Strength 60.0 - 339 kV/mm
1520 - 8610 kV/in
Average value: 206 kV/mm Grade Count:56
Overview of materials for Polyimide, Thermoset Film
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Thermoset Film". Each property range of values reported is minimum and maximum values of appr..