Polymer Property : Dielectric Strength = 433 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 17.0 kV/mm
433 kV/in
ASTM D149
Saint-Gobain Meldin® 5001 Thermoplastic Bearing Material
General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin..
Dielectric Strength 17.0 kV/mm
433 kV/in
Dow Corning HV 1760/65 Silicone Rubber
65 Shore hardness high consistency silicone rubber with fast cure system and excellent tracking and erosion resistanceInformation provided by Dow Corning
Dielectric Strength 17.0 kV/mm
433 kV/in
Dow Corning HV 1760/80 SILICONE RUBBER NATURAL
80 Shore hardness high consistency silicone rubber with fast cure system and excellent tracking and erosion resistanceInformation provided by Dow Corning