Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 15.4 - 17.4 kV/mm | 391 - 441 kV/in | short time |
Bulk Molding Compounds BMC A50-EG Low Glass, Encapsulation Grade Molding Compound BMC A50-EG is a low glass, encapsulation grade material. It is well suited for injection, transfer or compression molding of intricate parts. Typical applications are motor armatures and coils.Inf.. |