Polymer Property : Dielectric Strength = 46.0 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 1.81 kV/mm
46.0 kV/in
ASTM D495
BNZ Materials Marinite® P High Temperature Structural Insulation
Oven dried formulations of BNZ boards are used in a variety of heat insulating processes, fire protection and machined parts. Selection is commonly based on a balance between strength and insulating..
Dielectric Strength 1.81 kV/mm
46.0 kV/in
0.1" gap
3M Fluorinert™ FC-40 Electronic Liquid
3M™ Fluorinert™ Liquid FC-40 is a non-conductive, thermally and chemically stable fluid ideal for single phase heat transfer fluid applications, especially in the electronics and semiconductor ind..