Material Notes:
Oven dried formulations of BNZ boards are used in a variety of heat insulating processes, fire protection and machined parts. Selection is commonly based on a balance between strength and insulating qualities. Examples include oven walls and linings, soldering insulation, fire doors, fire training burn buildings, cable trays, personnel protection, and as USCG-approved insulation for marine ships and off-shore rigs. Back-up insulation applications include ladles, torpedo cars and tundishes in the iron and steel industry, lime and cement plant rotary kilns, and aluminum die cast holding furnaces.Information provided by BNZ Materials Inc.
Physical Properties Metric English Comments
Density 0.961 g/cc
0.0347 lb/in³
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00960 GPa
1.39 ksi
Compressive Yield Strength 21.0 MPa

@Strain 5.00 %
3050 psi

@Strain 5.00 %
Thermal Properties Metric English Comments
Thermal Conductivity 0.160 W/m-K

@Temperature 204 °C
1.11 BTU-in/hr-ft²-°F

@Temperature 399 °F
0.170 W/m-K

@Temperature 316 °C
1.18 BTU-in/hr-ft²-°F

@Temperature 601 °F
0.170 W/m-K

@Temperature 427 °C
1.18 BTU-in/hr-ft²-°F

@Temperature 801 °F
0.170 W/m-K

@Temperature 538 °C
1.18 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Shrinkage 0.60 %

@Temperature 649 °C,
Time 86400 sec
0.60 %

@Temperature 1200 °F,
Time 24.0 hour
Length/width
2.1 %

@Temperature 649 °C,
Time 86400 sec
2.1 %

@Temperature 1200 °F,
Time 24.0 hour
Thickness
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+8 ohm-cm
5.00e+8 ohm-cm
ASTM D257
Dielectric Strength 1.81 kV/mm
46.0 kV/in
ASTM D495
Processing Properties Metric English Comments
Moisture Content 3.0 %
3.0 %
Descriptive Properties Value Comments
Screw Holding Strength 227 kg
at 7/8" penetration