Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 14.7 - 18.9 kV/mm | 373 - 480 kV/in | Average value: 16.9 kV/mm Grade Count:9 |
Overview of materials for Epoxy, High Temperature This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val.. |