Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 49.6 kV/mm | 1260 kV/in | ASTM D149 |
ExxonMobil LD 419.MV Wire & Cable Resin
(discontinued **) LD 419.MV is a LDPE designed for wire and cable applications and is suitable for making crosslinkable compounds for medium voltage insulation.Information provided by ExxonMobil Chemical |