Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 5.51 kV/mm | 140 kV/in | ASTM D149 |
3M 4516 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |
|||
Dielectric Strength | 5.51 kV/mm | 140 kV/in | ASTM D1000 |
3M Bumpon™ SJ5904 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Dielectric Strength | 5.51 kV/mm | 140 kV/in | ASTM D1000 |
3M Bumpon™ SJ5908 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Dielectric Strength | 5.51 kV/mm | 140 kV/in | ASTM D1000 |
3M Bumpon™ SJ5916 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |