Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Bumpon™ SJ5916 Resilient Rollstock

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Bumpon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Bumpon™ SJ5916 Resilient Rollstock.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Physical Properties Metric English Comments
Density 0.640 g/cc
0.0231 lb/in³
Thickness 1570 microns
62.0 mil
Mechanical Properties Metric English Comments
Hardness, Shore M 40
40
Polyurethane, medium foam
Tensile Strength at Break 0.830 MPa
120 psi
Die A; ASTM D412
Elongation at Break 100 %
100 %
Die A; ASTM D412
Coefficient of Friction >= 1.0
>= 1.0
Stainless Steel, Kinetic
>= 1.0
>= 1.0
Glass, Kinetic
0.80 - 1.4
0.80 - 1.4
Formica laminate, Kinetic
0.80 - 1.4
0.80 - 1.4
Wood, Kinetic
Peel Strength 0.526 kN/m
3.00 pli
90°, Adhesion to Polypropylene
1.93 kN/m
11.0 pli
90°, Adhesion to Polystyrene
4.38 kN/m
25.0 pli
90°, Adhesion to ABS
4.38 kN/m
25.0 pli
90°, Adhesion to Stainless Steel
4.38 kN/m
25.0 pli
90°, Adhesion to Aluminum
Taber Abrasion, mg/1000 Cycles 1.8 - 2.0
1.8 - 2.0
H18, 1 kg; ASTM C501
Compression Set 12 %
12 %
ASTM D1056
14 %
14 %
50% deflection; ASTM D1056
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 52.0 °C
126 °F
Application
66.0 °C
151 °F
Service
107 °C
225 °F
Intermittent Exposure
Minimum Service Temperature, Air -34.0 °C
-29.2 °F
Service
5.00 °C
41.0 °F
Application
Electrical Properties Metric English Comments
Dielectric Strength 5.51 kV/mm
140 kV/in
ASTM D1000
Descriptive Properties Value Comments
Adhesive Type A-20 (acrylic)
Appearance Black
Users viewing this material also viewed the following: